Andy Grant
Well-known member
My epoxy and fiberglass should arrive this Wednesday for my sculling float. It is strip built. My plan is:
1. seal coat with epoxy
2. lay down glass over hull and roughly cut to size (a couple inches big)
3. wet out glass with epoxy with a chip brush and squeegee off excess.
4. add another layer of epoxy to smooth.
Is this the right process? I have never really glassed anything before.
1. seal coat with epoxy
2. lay down glass over hull and roughly cut to size (a couple inches big)
3. wet out glass with epoxy with a chip brush and squeegee off excess.
4. add another layer of epoxy to smooth.
Is this the right process? I have never really glassed anything before.